Total PPR 6575 Polypropylene, Random Copolymer, Film Grade

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Total Atofina
Trade Name PPR
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPR 6575 Polypropylene, Random Copolymer, Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Color. Low catalyst residuals in TOTAL Petrochemicals 6575 polypropylene results in improved color stability.Clarity/Impact. The random copolymer structure of 6575 improves its clarity and resiliency over conventional homopolymer films.FDA. 6575 complies with all applicable FDA regulations for food contact applications.Recommended Applications. 6575 is recommended for use in manufacture of packaging films that require improved optical and resiliency or special surface attributes.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D1505
Water Vapor Transmission 10.9 g/m²/day

@Temperature 37.8 °C
0.700 g/100 in²/day

@Temperature 100 °F
90% RH; ASTM F1249-90
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.3 MPa
7000 psi
non-oriented film; ASTM D882
Elongation at Break 500 %
500 %
ASTM D882
Dart Drop 1.38 g/micron
35.0 g/mil
ASTM D1709
Thermal Properties Metric English Comments
Melting Point 148 °C
298 °F
DSC
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
ASTM D1003
Gloss 80 %
80 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 232 - 274 °C
450 - 525 °F