Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PPR 6523WZ Polypropylene, Nucleated Random Copolymer for Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Total Atofina
Trade Name PPR
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPR 6523WZ Polypropylene, Nucleated Random Copolymer for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact - 6523WZ produces molded parts with improved impact compared with parts molded from homopolymer polypropylene.Antistat - 6523WZ contains an antistat to help protect molded parts from dust accumulation.FDA - 6523WZ complies with all applicable FDA regulations for food contact applications.Recommended Applications. - 6523WZ is recommended for injection molding housewares, caps and closures and other items calling for a combination of good impact and easy mold release.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D1505
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238, L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785A
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Tensile Modulus 1.30 GPa
189 ksi
ASTM D638
Flexural Modulus 1.20 GPa
174 ksi
ASTM D790
Izod Impact, Notched 0.450 J/cm
0.843 ft-lb/in
ASTM D256A
Izod Impact, Unnotched NB
NB
ASTM D256A
Thermal Properties Metric English Comments
Melting Point 149 °C
300 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C
181 °F
ASTM D648