Material Notes:
ATOFINA Polypropylene PPH 9040 is a nucleated homopolymer. PPH 9040 is characterized by an improved rigidity and high clarity .ApplicationATOFINA Polypropylene PPH 9040 is suitable for the injection molding of packaging containers, toys, domestic appliances, garden furniture, and caps and closures. Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ISO 2039-2
Tensile Strength, Yield 36.0 MPa
5220 psi
ISO 527-2
Elongation at Yield 8.0 %
8.0 %
ISO 527-2
Tensile Modulus 2.00 GPa
290 ksi
ISO 527-2
Flexural Modulus 1.90 GPa
276 ksi
ISO 527-2
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
120°C per hour; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
120°C per hour; ISO 75-2
Vicat Softening Point 97.0 °C
207 °F
50N-50°C per hour; ISO 306
153 °C
307 °F
10N-50°C per hour; ISO 306