Material Notes:
Polypropylene 3576 BB is recommended for use in non-oriented cast films processes. It contains an optimized level of slip and anti-block additives.3576 BB is intended for food, magazine or textile packaging, for lamination films as well as for stationary supplies.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Melt Flow 8.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Antiblock Level 1800 ppm
1800 ppm
SiO2
Slip Level 1800 ppm
1800 ppm
Erucamide
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Flexural Modulus 1.40 GPa
203 ksi
ASTM D790
Izod Impact, Notched 0.350 J/cm
0.656 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
DSC
Vicat Softening Point 153 °C

@Load 1.02 kg
307 °F

@Load 2.25 lb
ASTM D1525
Descriptive Properties Value Comments
Isotacticity Index (%) 97.5