Total PPH 3150 Polypropylene, Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Total Atofina
Trade Name PPH
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH 3150 Polypropylene, Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polypropylene PPH 3150 is a modified homopolymer polypropylene with a Melt Flow index of 2 g/10 min.Polypropylene PPH 3150 is intended for the production at very high speed of flat bioriented films for food packaging. It does not contain any slip or antistatic agents and is Calcium Stearate free.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ISO 1183
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ISO 2039-2
Tensile Strength, Yield 33.0 MPa
4790 psi
ISO 527-2
Elongation at Yield 10 %
10 %
ISO 527-2
Tensile Modulus 1.40 GPa
203 ksi
ISO 527-2
Flexural Modulus 1.30 GPa
189 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 162 °C
324 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
120°C per hour; ISO 752
Vicat Softening Point 85.0 °C

@Load 5.10 kg
185 °F

@Load 11.2 lb
50°C per hour; ISO 306
150 °C

@Load 1.02 kg
302 °F

@Load 2.25 lb
50°C per hour; ISO 306