Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PPC 7652 Polypropylene, Heterophasic Copolymer, Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Total Atofina
Trade Name PPC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPC 7652 Polypropylene, Heterophasic Copolymer, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polypropylene PPC 7652 is a nucleated and antistatic heterophasic copolymer with a Melt Flow index of 16 g/10 min.Polypropylene PPC 7652 is a medium flow grade intended for a wide range of injection molding applications including battery cases, electrical appliance housings, toys, closures and lids.Polypropylene PPC 7652 has been specially formulated to give antistatic performance.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ISO 1183
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ISO 2039-2
Tensile Strength, Yield 26.0 MPa
3770 psi
ISO 527-2
Elongation at Yield 10 %
10 %
ISO 527-2
Tensile Modulus 1.45 GPa
210 ksi
ISO 527-2
Flexural Modulus 1.35 GPa
196 ksi
ISO 178
Izod Impact, Notched (ISO) 5.50 kJ/m²

@Temperature -20.0 °C
2.62 ft-lb/in²

@Temperature -4.00 °F
ISO 180
9.00 kJ/m²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact, Notched 0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
ISO 179
1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
120°C per hour; ISO 752
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C
126 °F
120°C per hour; ISO 752
Vicat Softening Point 75.0 °C

@Load 5.10 kg
167 °F

@Load 11.2 lb
50°C per hour; ISO 306
145 °C

@Load 1.02 kg
293 °F

@Load 2.25 lb
50°C per hour; ISO 306
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved