Total PPC 5571 Polypropylene, Impact Copolymer Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Total Atofina
Trade Name PPC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPC 5571 Polypropylene, Impact Copolymer Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TOTAL Petrochemicals Polypropylene 5571 is a high impact copolymer with a Melt Flow index of 7 g/10 min.TOTAL Polypropylene 5571 is characterized by significantly improved impact resistance, while maintaining excellent antistatic properties and good processability.Total Polypropylene 5571 has been developed specifically for the injection molding of baskets, pails, toys and any articles requiring extra toughness.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D1505
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Izod Impact, Notched 0.700 J/cm

@Temperature -20.0 °C
1.31 ft-lb/in

@Temperature -4.00 °F
ASTM D256
1.88 J/cm

@Temperature 23.0 °C
3.52 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 160 - 165 °C
320 - 329 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
pressure unspecified; ASTM D648
Vicat Softening Point 148 °C
298 °F
ASTM D1525