Total PPC 4720 WZ Polypropylene, Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Total Atofina
Trade Name PPC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPC 4720 WZ Polypropylene, Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ATOFINA 4720 is an impact copolymer. 4720 is characterized by a high fluidity offering a combination of east of processing and good mechanical properties.ApplicationATOFINA 4720 has been formulated for the manufacture of thin-walled containers and household articles. Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 25 g/10 min
25 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
ASTM D 790
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
0.400 J/cm

@Temperature -20.0 °C
0.749 ft-lb/in

@Temperature -4.00 °F
ASTM D256
Charpy Impact Unnotched 0.900 J/cm²
4.28 ft-lb/in²
Notched/Unnotched not specified; ASTM DIN53453
0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
Notched/Unnotched not specified; ASTM DIN53453
Thermal Properties Metric English Comments
Melting Point 160 - 165 °C
320 - 329 °F
ATOFINA Method
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ASTM D648
Vicat Softening Point 148 °C
298 °F
ASTM D1525