Material Notes:
FINATHENE® MS 201 B N is a high density polyethylene produced by a low pressure slurry polymerization process. FINATHENE® MS 201 B N has been developed for the blow molding of Plastic Fuel Tanks and automotive technical parts.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ISO 1183
Environmental Stress Crack Resistance >= 360 hour
>= 360 hour
ASTM D1693 cond. B 100% lgepal
Thermal Stress Crack Resistance >= 250 hour
>= 250 hour
ASTM D 1693
High Load Melt Index 8.0 g/10 min

@Load 21.6 kg
8.0 g/10 min

@Load 47.6 lb
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO 527
Elongation at Break >= 600 %
>= 600 %
ISO 527
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
Izod Impact, Notched 6.41 J/cm

@Thickness 3.17 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 127 °C
260 °F
ASTM D3417