Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Lumicene® M6040 Metallocene High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Total Atofina
Trade Name Lumicene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lumicene® M6040 Metallocene High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lumicene® M6040 is a second generation metallocene high density polyethylene with very good organoleptic properties, dimensional stability, rigidity and processability.It is especially suited for the production of caps & closures for non-carbonated drinks by compression molding. Other typical applications include caps & closures for cosmetics and general purpose injection-molded articles.This grade does not contain a slip agent.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ISO 1183
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133/D
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4210 psi
ISO 527
Tensile Modulus 1.30 GPa
189 ksi
ISO 527
Thermal Properties Metric English Comments
Melting Point 133 °C
271 °F
ISO 11357
Processing Properties Metric English Comments
Processing Temperature <= 250 °C
<= 482 °F