Total Lacqtene® FD 0270 LDPE, blown film, compounding, injection molding  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lacqtene® FD 0270 LDPE, blown film, compounding, injection molding  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low density radical polyethylene made by high pressure process. Temperature profile (°C) for injection molding: 200 to 260Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ISO 1183
Melt Flow 2.1 g/10 min
2.1 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ISO 868
Tensile Strength at Break 14.0 MPa
2030 psi
ISO 527
Tensile Strength, Yield 12.0 MPa
1740 psi
ISO 527
Elongation at Break 650 %
650 %
ISO 527
Modulus of Elasticity 0.240 GPa
34.8 ksi
ISO 5527
Dart Drop Test 140 g
0.309 lb
50µ; ISO 7765-1
Thermal Properties Metric English Comments
Melting Point 112 °C
234 °F
ISO 11357-3
Vicat Softening Point 96.0 °C
205 °F
ISO 306
Optical Properties Metric English Comments
Haze 9.0 %
9.0 %
50µ; ASTM D 1003
Descriptive Properties Value Comments
Food Status This material conforms to both European and American Food contact regulations.
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved