Material Notes:
LACQTENE® 6002 FLG 42 is a medium density polyethylene resin with hexene as comonomer. This shows a broad molecular weight distribution ensuring outstanding processability. LACQTENE® 6002 FLG 42 has been especially dedicated to film applications where a lower gel content and a higher rigidity are required, particularly in blend and coextrusion with LLDPE and LDPE.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D 792
Melt Flow 0.20 g/10 min

@Load 2.16 kg
0.20 g/10 min

@Load 4.76 lb
ISO 1133
0.80 g/10 min

@Load 5.00 kg
0.80 g/10 min

@Load 11.0 lb
ISO 1133
High Load Melt Index 16.5 g/10 min

@Load 21.6 kg
16.5 g/10 min

@Load 47.6 lb
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 32.0 MPa
4640 psi
ISO R527
Elongation at Break 830 %
830 %
ISO R527
Flexural Modulus 0.850 GPa
123 ksi
Dart Drop Test 65.0 g
0.143 lb
ASTM D 1709 A
Thermal Properties Metric English Comments
Melting Point 126 °C
259 °F
ISO 11357-3
Vicat Softening Point 121 °C
250 °F
ISO 306
Optical Properties Metric English Comments
Haze 55 %
55 %
ASTM D 1003
Gloss 10 %
10 %
45 degrees; ASTM D 2457
Descriptive Properties Value Comments
Food Status This material is formulated to comply with most requirements of the food packaging regulations