Total Lacqtene® 2001 TBK 40 HDPE pipe  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lacqtene® 2001 TBK 40 HDPE pipe  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LACQTENE® 2002 TBK 40 is a medium density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2002 TBK 40 is a black compound especially developed for pressure pipe for gas and potable water. LACQTENE® 2002 TBK 40 may be used for irrigation pipe and geomembranes.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ISO 1183
Oxidative Induction Time (OIT) >= 20 min
>= 20 min
200°C; EN 728
Melt Flow 0.20 g/10 min

@Load 2.16 kg
0.20 g/10 min

@Load 4.76 lb
ISO 1133
0.75 g/10 min

@Load 5.00 kg
0.75 g/10 min

@Load 11.0 lb
ISO 1133
High Load Melt Index 18 g/10 min

@Load 21.6 kg
18 g/10 min

@Load 47.6 lb
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ISO 868
Tensile Strength, Yield 22.0 MPa
3190 psi
ISO 527-2
Elongation at Break >= 600 %
>= 600 %
ISO 527-2
Flexural Modulus 0.750 GPa
109 ksi
ISO 178
Izod Impact, Notched (ISO) 17.5 kJ/m²

@Temperature 23.0 °C
8.33 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Melting Point 127 °C
261 °F
ISO 3146
Vicat Softening Point 118 °C
244 °F
ISO 306
Descriptive Properties Value Comments
Food Status This material conforms to both European and American Food contact regulations.