Total Lacqrene® 814(AS) High Impact Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lacqrene® 814(AS) High Impact Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LACQRENE® 814 is a high impact, flame retardant polystyrene, free from PBDPE and with excellent thermal stability.ApplicationCovers for electrical equipment, Office equipment: copiers, faxInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D1505
Water Absorption <= 0.10 %
<= 0.10 %
ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 200 °C
10 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238G
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.6 MPa
3270 psi
ASTM D638
Elongation at Break 45 %
45 %
ASTM D638M
Flexural Modulus 1.96 GPa
284 ksi
ASTM D790
Izod Impact, Notched 0.883 J/cm
1.65 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Vicat Softening Point 88.0 °C
190 °F
50N (T° increase = 5°C/h); ASTM D1525B
97.0 °C
207 °F
10N (T° increase = 50°C/h); ASTM D1525A