Total HDPE 6280 High Density Polyethylene, Injection Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Total Atofina
Trade Name HDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total HDPE 6280 High Density Polyethylene, Injection Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics:Excellent stiffnessExcellent surface appearanceGood warp resistanceExcellent impact resistanceASTM D 1248 - Type III, Class A, Category 3FDA CompliantApplications:Dairy cratesPalletsMaterial handling containersTotesTraysSuitable for food packagingInformation provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
ESCR 10% Igepal® >= 10 hour
>= 10 hour
ASTM D1693, Cond. B
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Modulus 1.59 GPa
230 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 129 °C
265 °F
ASTM D3417
Brittleness Temperature -80.0 °C
-112 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 204 - 260 °C
400 - 500 °F
Injection Molding