Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Finathene® WR 201 B N HDPE blow molding  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finathene® WR 201 B N HDPE blow molding  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FINATHENE® WR 201 B N is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® WR 201 B N has been developed for the blow molding of Plastic Fuel Tanks and automotive technical parts. FINATHENE® WR 201 B N is suitable for the most common barrier treatments. The material specific characteristics allow to achieve outstanding tank properties, including crash test and fire resistance, with a substantial net weight reduction of the Plastic Fuel Tank.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.9495 g/cc
0.03430 lb/in³
ISO 1183
Environmental Stress Crack Resistance >= 360 hour
>= 360 hour
ASTM D1693 cond. B 100% lgepal
Thermal Stress Crack Resistance >= 250 hour
>= 250 hour
ASTM D 1693
High Load Melt Index 8.0 g/10 min

@Load 21.6 kg
8.0 g/10 min

@Load 47.6 lb
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527
Elongation at Yield 11 %
11 %
ISO 527
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
Impact Test 20.0 J
14.8 ft-lb
Multiaxial, @ ULT, deflection = 14 mm; ASTM D 3763
Thermal Properties Metric English Comments
Melting Point 127 °C
261 °F
ASTM D3417