Total Finathene® DF 210 HDPE resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , MDPE , Medium Density Polyethylene (MDPE), Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finathene® DF 210 HDPE resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Irrigation tape and tubingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.937 g/cc
0.0339 lb/in³
ASTM D 792
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
ASTM D1693 cond. B 100% lgepal
Melt Flow 0.28 g/10 min

@Load 2.16 kg
0.28 g/10 min

@Load 4.76 lb
ASTM D 1238
High Load Melt Index 20 g/10 min

@Load 21.6 kg
20 g/10 min

@Load 47.6 lb
ASTM D 1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD >= 21.4 MPa
>= 3100 psi
ASTM D 882 A
Film Tensile Strength at Yield, TD >= 21.4 MPa
>= 3100 psi
ASTM D 882 A
Film Elongation at Break, MD 500 %
500 %
ASTM D 882 A
Film Elongation at Break, TD 600 %
600 %
ASTM D 882 A
Elmendorf Tear Strength MD 50 g
50 g
ASTM D 1922
Elmendorf Tear Strength TD 500 g
500 g
ASTM D 1922
Dart Drop Test 130 g
0.287 lb
ASTM D 1709 A
Film Tensile Strength at Break, MD 42.1 MPa
6100 psi
ASTM D 882A
Film Tensile Strength at Break, TD 42.1 MPa
6100 psi
ASTM D 882A
Thermal Properties Metric English Comments
Melting Point 126 °C
259 °F
ASTM D3417