Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Toho Tenax Besfight® G30-700 24K HTA-7D F402 Continuous Filament Carbon Fiber

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Toho Tenax Co., Ltd.
Trade Name Besfight®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Toho Tenax Besfight® G30-700 24K HTA-7D F402 Continuous Filament Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Standard Modulus; Wide Band; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon Fibers, a wholly owned subsidiary of Toho Tenax Co., Ltd.
Physical Properties Metric English Comments
Density 1.79 g/cc
0.0647 lb/in³
Fiber Count 16560 dtex
14900 denier
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 5100 MPa
740000 psi
Elongation at Break 2.1 %
2.1 %
Tensile Modulus 241 GPa
35000 ksi
Electrical Properties Metric English Comments
Electrical Resistivity 0.00150 ohm-cm
0.00150 ohm-cm
Descriptive Properties Value Comments
Filament Diameter 7 µm
Size Level 1.6%
Copyright © lookpolymers.com All Rights Reserved