Tipco Tipcolite® TX 321 Phenolic Compound, Wood Flour & Minerals, having Soft Flow & High Electrical Properties

Category Polymer , Thermoset , Phenolic
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolite® TX 321 Phenolic Compound, Wood Flour & Minerals, having Soft Flow & High Electrical Properties.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Soft Flow Phenolic Compound, Reinforced with Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MouldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Apparent Bulk Density 0.630 g/cc
0.0228 lb/in³
TRM-37
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 45.0 MPa
6530 psi
ASTM D638
Flexural Yield Strength 75.0 MPa
10900 psi
ASTM D790
Izod Impact, Unnotched (ISO) 2.40 kJ/m²
1.14 ft-lb/in²
ASTM D256
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
ASTM D257
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
ASTM D257
Dielectric Strength 9.00 kV/mm
229 kV/in
ASTM D149