Tipco Tipcolite® TPF 1315 - Unreinforced Phenolic Resin having 22 mm Norton Flow with 10% Hexamine

Category Polymer , Thermoset , Phenolic
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolite® TPF 1315 - Unreinforced Phenolic Resin having 22 mm Norton Flow with 10% Hexamine.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unreinforced Phenolic Resin having 22mm Norton Flow, in Powder FormApplications: Foundry & RefractoryProcessing: Castings & ShellsInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Spiral Flow 2.20 cm
0.866 in
Thermal Properties Metric English Comments
Melting Point 95.0 °C
203 °F
TRN-14