Tipco Tipcolite® TPF 1113 - Unreinforced Thermoset Phenolic Resin, 55 mm Norton Flow with 5% Hexamine

Category Polymer , Thermoset , Phenolic
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolite® TPF 1113 - Unreinforced Thermoset Phenolic Resin, 55 mm Norton Flow with 5% Hexamine.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unreinforced Phenolic Resin having 55mm Norton Flow, in Powder FormApplications: General PurposeProcessing: General PurposeInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Spiral Flow 5.50 cm
2.17 in
Thermal Properties Metric English Comments
Melting Point 95.0 °C
203 °F
TRN-14