Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tipco Tipcolite® TEL 211 Phenolic Compound, Glass & Nylon Fibers, Soft Flow & Low Shrinkage

Category Polymer , Thermoset , Phenolic
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolite® TEL 211 Phenolic Compound, Glass & Nylon Fibers, Soft Flow & Low Shrinkage.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Soft Flow Phenolic Compound, Reinforced with Glass & Nylon FibresApplications: Automotives & ElectricalProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Apparent Bulk Density 0.450 g/cc
0.0163 lb/in³
TRM-37
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Flexural Yield Strength 78.0 MPa
11300 psi
ASTM D790
Izod Impact, Notched (ISO) 2.20 kJ/m²
1.05 ft-lb/in²
ASTM D256
Electrical Properties Metric English Comments
Volume Resistivity 3.16e+11 ohm-cm
3.16e+11 ohm-cm
ASTM D257
Surface Resistance 3.16e+11 ohm
3.16e+11 ohm
ASTM D257
Dielectric Strength 6.50 kV/mm
165 kV/in
ASTM D149