Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® SEB 400 - 40% Chemically Coupled Glass Fibers Polypropylene Homopolymer with High Heat Stability.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 113 MPa
16400 psi
ASTM D638
Elongation at Break >= 4.0 %
>= 4.0 %
ASTM D638
Flexural Yield Strength 167 MPa
24200 psi
ASTM D790
Flexural Modulus 7.80 GPa
1130 ksi
ASTM D790
Izod Impact, Notched (ISO) 19.0 kJ/m²
9.04 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 158 °C
316 °F
ASTM D648