Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tipco Tipcolene® PPH-OIT - Unfilled Polypropylene Homopolymer Compound with Copper Inhibitor (Metal Deactivator)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® PPH-OIT - Unfilled Polypropylene Homopolymer Compound with Copper Inhibitor (Metal Deactivator).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PP Homopolymer with Copper Inhibitor (Metal De-activator)Applications: Automotives & ElectricalProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Linear Mold Shrinkage 0.019 cm/cm
0.019 in/in
ASTM D955
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Elongation at Break >= 50 %
>= 50 %
ASTM D638
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ASTM D256
Users viewing this material also viewed the following: