Tipco Tipcolene® ISRH 35 NF - 20% Talc/Mineral Reinforced Polypropylene Homopolymer, High Flow

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® ISRH 35 NF - 20% Talc/Mineral Reinforced Polypropylene Homopolymer, High Flow.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Mineral Reinforced, PP HomopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Melt Flow 30 g/10 min
30 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 88
88
Tensile Strength, Yield 21.5 MPa
3120 psi
ASTM D638
Elongation at Break >= 5.0 %
>= 5.0 %
ASTM D638
Flexural Yield Strength 34.0 MPa
4930 psi
ASTM D790
Flexural Modulus 2.15 GPa
312 ksi
ASTM D790
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ASTM D648