Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tipco Tipcolene® FX 6000 - UL94-V0 Flame Retardant & Mineral Reinforced Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® FX 6000 - UL94-V0 Flame Retardant & Mineral Reinforced Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mineral Reinforced V0 Flame Retardant PP CopolymerApplications: Modular SwitchesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Elongation at Break >= 50 %
>= 50 %
ASTM D638
Flexural Yield Strength 29.5 MPa
4280 psi
ASTM D790
Flexural Modulus 1.96 GPa
284 ksi
ASTM D790
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Oxygen Index 28 %
28 %
ISO 4589
Users viewing this material also viewed the following: