Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tipco Tipcolene® FX 4002 - UL94-V2 Flame Retardant Polypropylene Copolymer Compound with High Impact Strength

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® FX 4002 - UL94-V2 Flame Retardant Polypropylene Copolymer Compound with High Impact Strength.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
V-2 Flame Retardant PP Copolymer with High Impact StrengthApplications: Battery LidsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.5 MPa
2970 psi
ASTM D638
Elongation at Break >= 75 %
>= 75 %
ASTM D638
Flexural Yield Strength 28.0 MPa
4060 psi
ASTM D790
Flexural Modulus 1.37 GPa
199 ksi
ASTM D790
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Oxygen Index 24 %
24 %
ISO 4589
Copyright © lookpolymers.com All Rights Reserved