Tipco Tipcolene® FPTC 30 HG - 30% Talc & Calcium Carbonate Polypropylene Homopolymer, High Gloss & Stiffness

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® FPTC 30 HG - 30% Talc & Calcium Carbonate Polypropylene Homopolymer, High Gloss & Stiffness.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Talc+Calcium Reinforced PP Homopolymer with High GlossApplications: Furniture & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Break >= 30 %
>= 30 %
ASTM D638
Flexural Yield Strength 46.0 MPa
6670 psi
ASTM D790
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
Izod Impact, Notched (ISO) 5.50 kJ/m²
2.62 ft-lb/in²
ASTM D256