Tipco Tipcolene® FPC 40 - 40% Calcium Carbonate Reinforced Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® FPC 40 - 40% Calcium Carbonate Reinforced Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% Calcium Carbonate Filled PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.5 MPa
3550 psi
ASTM D638
Elongation at Break >= 50 %
>= 50 %
ASTM D638
Flexural Yield Strength 45.0 MPa
6530 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ASTM D256