Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tipco Tipcolene® CR 8229 - 20% Talc/Mineral Reinforced Polypropylene Copolymer Compound with Controlled Rheology

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® CR 8229 - 20% Talc/Mineral Reinforced Polypropylene Copolymer Compound with Controlled Rheology.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Mineral Reinforced, High Flow & Controlled Rheology PP CopolymerApplications: Automotive Door TrimsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Melt Flow 18 g/10 min
18 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Break >= 30 %
>= 30 %
ASTM D638
Flexural Yield Strength 40.0 MPa
5800 psi
ASTM D790
Flexural Modulus 2.25 GPa
326 ksi
ASTM D790
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C