Tipco Megabatch® MD 3220 LLDPE based Metal De-Activator Masterbatch

Category Polymer
Manufacturer Tipco Industries Ltd., India
Trade Name Megabatch®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Megabatch® MD 3220 LLDPE based Metal De-Activator Masterbatch.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Metal De-Activator (Cu-Inhibitor) Masterbatch in LLDPEApplications: General PurposeProcessing: Injection & ExtrusionInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Apparent Bulk Density 0.600 g/cc
0.0217 lb/in³
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238