ThyssenKrupp XABO® 1100 Structural Steel

Category Metal , Ferrous Metal
Manufacturer ThyssenKrupp
Trade Name XABO®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ThyssenKrupp XABO® 1100 Structural Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This Material Specification applies to liquid-quenched and tempered heavy plates from 4 up to 40 mm in thickness, made of the high-strength special structural steel XABO® 1100.Application: The steels may be used for welded constructions of all kinds such as transport vehicles, mobile cranes, hoistings, mining equipment etc.Information Provided by Thyssen Krupp
Mechanical Properties Metric English Comments
Tensile Strength at Break 1200 - 1500 MPa
174000 - 218000 psi
Tensile Strength, Yield >= 1100 MPa
>= 160000 psi
Elongation at Break >= 8.0 %
>= 8.0 %
Charpy Impact 27.0 J

@Temperature -40.0 °C
19.9 ft-lb

@Temperature -40.0 °F
Transverse
30.0 J

@Temperature -40.0 °C
22.1 ft-lb

@Temperature -40.0 °F
Longitudinal
Component Elements Properties Metric English Comments
Aluminum, Al <= 1.5 %
<= 1.5 %
Carbon, C <= 0.20 %
<= 0.20 %
Chromium, Cr <= 1.5 %
<= 1.5 %
Manganese, Mn <= 1.7 %
<= 1.7 %
Molybdenum, Mo <= 0.70 %
<= 0.70 %
Nickel, Ni <= 2.5 %
<= 2.5 %
Phosphorous, P <= 0.020 %
<= 0.020 %
Silicon, Si <= 0.50 %
<= 0.50 %
Sulfur, S <= 0.0050 %
<= 0.0050 %
Vanadium, V <= 0.12 %
<= 0.12 %