Thermoseal Miliam Mica PPS 300 Laminate

Category Ceramic , Oxide
Manufacturer Thermoseal Inc.
Trade Name Miliam Mica
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Thermoseal Miliam Mica PPS 300 Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type PSSHigh Quality Mica SheetLaminated on Pegged Stainless Steel Insert All Milam laminates are suitable for use in hot, dry gas applications such as exhaust manifolds, turbines, turbo chargers and air heat exchangers.Information provided by Thermoseal Inc.
Physical Properties Metric English Comments
Loss On Ignition <= 15 %
<= 15 %
DIN 52911
Thickness 1588 microns
62.52 mil
+/- 5% of nominal thickness
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 900.0 °C
1652 °F
Descriptive Properties Value Comments
Color Metallic Tan
Compressibility 18-23 percent
ASTM F36A
Gas Permeability >100 ml/min
DIN 3535/6
Pressure <14,503 psi
Recovery 48-53 percent
ASTM F36A
Stress Relaxation 2900 psi
40 MPa/300°C, DIN 52913
4351 psi
50 MPa/300°C, DIN 52913
Tang Insert Stainless Steel Thickness 0.004 in
AISI 316