Thermoseal Miliam Mica PPS 150 Laminate

Category Ceramic , Oxide
Manufacturer Thermoseal Inc.
Trade Name Miliam Mica
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Thermoseal Miliam Mica PPS 150 Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type PSSHigh Quality Mica SheetLaminated on Pegged Stainless Steel Insert All Milam laminates are suitable for use in hot, dry gas applications such as exhaust manifolds, turbines, turbo chargers and air heat exchangers.Information provided by Thermoseal Inc.
Physical Properties Metric English Comments
Loss On Ignition <= 5.0 %
<= 5.0 %
DIN 52911
Thickness 1500 microns
59.1 mil
+/- 5% of nominal thickness
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 900.0 °C
1652 °F
Descriptive Properties Value Comments
Color Metallic Tan
Compressibility 12-16 percent
ASTM F36A
Gas Permeability >100 ml/min
DIN 3535/6
Pressure <14,503 psi
Recovery 40-50 percent
ASTM F36A
Stress Relaxation 4641 psi
40 MPa/300°C, DIN 52913
5801 psi
50 MPa/300°C, DIN 52913
Tang Insert Stainless Steel Thickness 0.004 in
AISI 316