Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Thermoseal KLINGERSIL® C-5400 Neoprene Gasketing

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Thermoseal Inc.
Trade Name KLINGERSIL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Thermoseal KLINGERSIL® C-5400 Neoprene Gasketing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Synthetic FiberNeoprene BinderChemically StableGood Anti-Stick PropertiesInformation provided by Thermoseal Inc.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
ASTM F1315
Thickness 1588 microns
62.52 mil
Thickness tested
Electrical Properties Metric English Comments
Dielectric Strength 18.0 kV/mm
457 kV/in
ASTM D149-95a
Descriptive Properties Value Comments
Color White or Black
(Top/Bottom)
Compressibility 8 percent
ASTM F36J
Creep Relaxation 20 percent
1/32", ASTM F38B
Gas Permeability <0.5 ml/min
DIN 3535/6
Klinger Hot Compression Test 11 percent
Initial, Thickness Decrease 73°F (23°C)
21 percent
Additional, Thickness Decrease 572°F (300°C)
Leachable Chloride Content 500 ppm
FSA Method (Typical)
Recovery >50 percent
ASTM F36J
Sealability <0.2 ml/hr
1/32", ASTM F37A
Thickness Increase 0-10%
ASTM Fuel B, 5h/73°F (23°C)
0-5%
ASTM F146 after immersion in ASTM Oil 1, 5h/300°F (149°C)
0-5%
ASTM Fuel A, 5h/73°F (23°C)
5-20%
ASTM Oil IRM903, 5h/300°F (149°C)
Weight Increase <15%
ASTM F146 after immersion in Fuel B 5h/73°F (23°C)
Copyright © lookpolymers.com All Rights Reserved