Thermoseal KLINGERSIL® C-4439 Metal Reinforced Gasketing

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Thermoseal Inc.
Trade Name KLINGERSIL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Thermoseal KLINGERSIL® C-4439 Metal Reinforced Gasketing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fiberglass, Aramid & Inorganic FibersNitrile BinderHigh Temperature & StressVibrationGalvanized Low Carbon Steel InsertInformation provided by Thermoseal Inc.
Physical Properties Metric English Comments
Density 2.10 g/cc
0.0759 lb/in³
ASTM F1315
Thickness 1588 microns
62.52 mil
Thickness tested
Electrical Properties Metric English Comments
Dielectric Strength 10.0 kV/mm
254 kV/in
ASTM D149-95a
Descriptive Properties Value Comments
Color Red
(Top/Bottom)
Compressibility 8 percent
ASTM F36J
Creep Relaxation 20 percent
1/32", ASTM F38B
Klinger Hot Compression Test 4 percent
Additional, Thickness Decrease 572°F (300°C)
8 percent
Initial, Thickness Decrease 73°F (23°C)
Leachable Chloride Content 150 ppm
FSA Method (Typical)
Recovery >50 percent
ASTM F36J
Thickness Increase 0-5%
ASTM F146 after immersion in ASTM Oil 1, 5h/300°F (149°C)
0-5%
ASTM Oil IRM903, 5h/300°F (149°C)
0-5%
ASTM Fuel A, 5h/73°F (23°C)
5-10%
ASTM Fuel B, 5h/73°F (23°C)
Weight Increase <9%
ASTM F146 after immersion in Fuel B 5h/73°F (23°C)