Category | Ceramic |
Manufacturer | Thermal Ceramics |
Trade Name | Pyro-Bloc |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Thermal Ceramics Pyro-Bloc ZR Y and Y2 Modules.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.160 g/cc | 0.00578 lb/in³ | Available in multiple densities from manufacturer |
0.192 g/cc | 0.00694 lb/in³ | Available in multiple densities from manufacturer | |
0.240 g/cc | 0.00867 lb/in³ | Available in multiple densities from manufacturer | |
Thickness | 3000 - 12000 microns | 118 - 472 mil |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0706 W/m-K @Temperature 260 °C |
0.490 BTU-in/hr-ft²-°F @Temperature 500 °F |
15 pcf; ASTM C201 |
0.0720 W/m-K @Temperature 260 °C |
0.500 BTU-in/hr-ft²-°F @Temperature 500 °F |
12 pcf; ASTM C201 | |
0.0749 W/m-K @Temperature 260 °C |
0.520 BTU-in/hr-ft²-°F @Temperature 500 °F |
10 pcf; ASTM C201 | |
0.121 W/m-K @Temperature 538 °C |
0.840 BTU-in/hr-ft²-°F @Temperature 1000 °F |
15 pcf; ASTM C201 | |
0.138 W/m-K @Temperature 538 °C |
0.960 BTU-in/hr-ft²-°F @Temperature 1000 °F |
12 pcf; ASTM C201 | |
0.150 W/m-K @Temperature 538 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 1000 °F |
10 pcf; ASTM C201 | |
0.206 W/m-K @Temperature 816 °C |
1.43 BTU-in/hr-ft²-°F @Temperature 1500 °F |
15 pcf; ASTM C201 | |
0.239 W/m-K @Temperature 816 °C |
1.66 BTU-in/hr-ft²-°F @Temperature 1500 °F |
12 pcf; ASTM C201 | |
0.261 W/m-K @Temperature 816 °C |
1.81 BTU-in/hr-ft²-°F @Temperature 1500 °F |
10 pcf; ASTM C201 | |
0.316 W/m-K @Temperature 1090 °C |
2.19 BTU-in/hr-ft²-°F @Temperature 2000 °F |
15 pcf; ASTM C201 | |
0.353 W/m-K @Temperature 1090 °C |
2.45 BTU-in/hr-ft²-°F @Temperature 2000 °F |
12 pcf; ASTM C201 | |
0.388 W/m-K @Temperature 1090 °C |
2.69 BTU-in/hr-ft²-°F @Temperature 2000 °F |
10 pcf; ASTM C201 | |
Maximum Service Temperature, Air | 1340 °C | 2450 °F | Continuous |
1430 °C | 2600 °F | Rating |
Component Elements Properties | Metric | English | Comments |
---|---|---|---|
Al2O3 | 37.5 % | 37.5 % | |
SiO2 | 47 % | 47 % | |
ZrO2 | 15.5 % | 15.5 % |
Descriptive Properties | Value | Comments |
---|---|---|
Loss on Ignition | traces | |
Other Element Content | traces |