Material Notes:
MRI pressed fired shapes are used in a variety of alloy melt-pour systems. The pressed manufacture process meets the tight tolerance specifications required by end users. Precise size dies and detailed product inspection provide the user with a high-quality, dimensionally accurate refractory shape.MRI FS-85V 85% fused silica mix, ideal for extreme thermal shock conditions and ferrous/nonferrous metal contact.Features: Variety of available compositions in high alumina and fused silica. Extreme tight tolerance capabilities Low gas permeability to ferrous alloys Good non-wetting characteristics Excellent mechanical strength Proven performance in super alloy, investmentApplications: Standard size crucibles and liners for induction melting and investment casting Tundish nozzles - meet user demands on pour stream and pour speeds Gas atomized nozzles - for custom-designed atomizing powder metal systemsInformation provided by Thermal CeramicsData has not been recently verified. Please contact manufacturer for current information.