Category | Ceramic , Oxide , Silicon Oxide |
Manufacturer | Thermal Ceramics |
Trade Name | Kaowool |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Thermal Ceramics Kaowool S Blanket.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0640 g/cc | 0.00231 lb/in³ | Available in multiple densities from manufacturer |
0.0960 g/cc | 0.00347 lb/in³ | Available in multiple densities from manufacturer | |
0.128 g/cc | 0.00462 lb/in³ | Available in multiple densities from manufacturer | |
Thickness | 25000 - 50000 microns | 984 - 1970 mil |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0600 W/m-K @Temperature 260 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 500 °F |
8 pcf |
0.0700 W/m-K @Temperature 260 °C |
0.486 BTU-in/hr-ft²-°F @Temperature 500 °F |
6 pcf | |
0.0800 W/m-K @Temperature 260 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 500 °F |
4 pcf | |
0.130 W/m-K @Temperature 538 °C |
0.902 BTU-in/hr-ft²-°F @Temperature 1000 °F |
8 pcf | |
0.150 W/m-K @Temperature 538 °C |
1.04 BTU-in/hr-ft²-°F @Temperature 1000 °F |
6 pcf | |
0.190 W/m-K @Temperature 538 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 1000 °F |
4 pcf | |
0.230 W/m-K @Temperature 816 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 1500 °F |
8 pcf | |
0.270 W/m-K @Temperature 816 °C |
1.87 BTU-in/hr-ft²-°F @Temperature 1500 °F |
6 pcf | |
0.300 W/m-K @Temperature 982 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 1800 °F |
8 pcf | |
0.350 W/m-K @Temperature 982 °C |
2.43 BTU-in/hr-ft²-°F @Temperature 1800 °F |
6 pcf | |
0.360 W/m-K @Temperature 816 °C |
2.50 BTU-in/hr-ft²-°F @Temperature 1500 °F |
4 pcf | |
0.410 W/m-K @Temperature 1093 °C |
2.85 BTU-in/hr-ft²-°F @Temperature 1999 °F |
6 pcf | |
0.470 W/m-K @Temperature 982 °C |
3.26 BTU-in/hr-ft²-°F @Temperature 1800 °F |
4 pcf | |
Melting Point | 1760 °C | 3200 °F | |
Maximum Service Temperature, Air | 1090 °C | 2000 °F | Continuous |
1260 °C | 2300 °F | Rating |
Component Elements Properties | Metric | English | Comments |
---|---|---|---|
Al2O3 | 35 - 45 % | 35 - 45 % | |
Alkalis | 0.20 % | 0.20 % | |
CaO | 0.050 % | 0.050 % | |
Fe2O3 | 0.050 % | 0.050 % | |
MgO | 0.050 % | 0.050 % | |
Other | 0.00 - 3.0 % | 0.00 - 3.0 % | |
SiO2 | 50 - 54 % | 50 - 54 % | |
ZrO2 | 0.00 - 15 % | 0.00 - 15 % |
Descriptive Properties | Value | Comments |
---|---|---|
Water Leachable Elements on Surface of Fiber, PPM | Boron, 40 | |
Chlorine, <10 | ||
Fluorine, <5 | ||
Silicate, 125 | ||
Sodium, 40 | ||
Sulphur, 10 |