Thermal Ceramics Kaowool S Blanket Strip

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Thermal Ceramics
Trade Name Kaowool
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Thermal Ceramics Kaowool S Blanket Strip.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermal Ceramics Kaowool® Strip products are cut from either Kaowool Blanket, Blanket S, Cerablanket®, or Cerachem® Blanket. These products are available in many forms and lengths depending upon the application. They have low thermal conductivity, low heat storage capacity, and are extremely resistant to thermal shock.Blanket strip products are highly efficient insulators. These products have low shot content which allows more usable fiber for each insulating dollar. Blanket strip products have longer fibers which give them high tensile strength and resiliency to withstand vibration and physical abuse. Blanket strip products are self-supporting and will not separate, sag, or settle. Blanket strips are available in a wide variety of widths, thicknesses, densities, and chemistries. This allows the user to select the proper product form for an application with a minimum of scrap and labor to install the strip. Blanket strip products have a wide variety of uses including packing for modules, expansion joints, and gaskets.Features:Available in a wide variety of widths, thicknesses, and densities Available in all Blanket compositionsApplications: Expansion jointsHigh-temperature filtrationGaskets Acoustical service for missiles, rockets, and jet enginesHigh-temperature insulationPacking stripsInformation provided by Thermal CeramicsData has not been recently verified. Please contact manufacturer for current information.
Physical Properties Metric English Comments
Density 0.0480 - 0.128 g/cc
0.00173 - 0.00462 lb/in³
Thickness 12500 - 50000 microns
492 - 1970 mil
Thermal Properties Metric English Comments
Melting Point 1760 °C
3200 °F
Maximum Service Temperature, Air 1090 °C
2000 °F
Continuous
1090 °C
2000 °F
Rating
Component Elements Properties Metric English Comments
Al2O3 35 - 45 %
35 - 45 %
Other 0.00 - 3.0 %
0.00 - 3.0 %
SiO2 50 - 55 %
50 - 55 %
ZrO2 0.00 - 15 %
0.00 - 15 %
Descriptive Properties Value Comments
MgO Content trace
Water Leachable Elements on Surface of Fiber, PPM Boron, 40
Chlorine, <10
Fluorine, <5
Silicate, 125
Sodium, 40
Sulphur, 10