Thermal Ceramics Kaowool Blanket

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Thermal Ceramics
Trade Name Kaowool
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Thermal Ceramics Kaowool Blanket.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Kaowool blanket is produced from kaolin, a naturally occurring alumina-silica fire clay. Kaowool, the world’s most recognizable name in ceramic fiber blanket, is available in a wide variety of densities and sizes. Kaowool blanket offers excellent handleability and high temperature stability. This allows it to meet a wide range of hot face and backup insulation applications in furnaces, kilns and other equipment requiring high temperature heat containment.Military Specifications and Approvals:Mil-I-23128A- 3, 6 pcf blanketMil-I-24244- all blanketsMil-I-23128B- 6, 8 pcf blanketInformation provided by Thermal CeramicsData has not been recently verified. Please contact manufacturer for current information.
Physical Properties Metric English Comments
Density 0.0480 g/cc
0.00173 lb/in³
Available in multiple densities from manufacturer
0.0640 g/cc
0.00231 lb/in³
Available in multiple densities from manufacturer
0.0960 g/cc
0.00347 lb/in³
Available in multiple densities from manufacturer
0.128 g/cc
0.00462 lb/in³
Available in multiple densities from manufacturer
0.192 g/cc
0.00694 lb/in³
Available in multiple densities from manufacturer
Thickness 3125 - 50000 microns
123.0 - 1970 mil
Thermal Properties Metric English Comments
Thermal Conductivity 0.0600 W/m-K

@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 500 °F
8 pcf
0.0700 W/m-K

@Temperature 260 °C
0.486 BTU-in/hr-ft²-°F

@Temperature 500 °F
6 pcf
0.0800 W/m-K

@Temperature 260 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 500 °F
4 pcf
0.120 W/m-K

@Temperature 538 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 1000 °F
8 pcf
0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
6 pcf
0.190 W/m-K

@Temperature 538 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1000 °F
4 pcf
0.210 W/m-K

@Temperature 816 °C
1.46 BTU-in/hr-ft²-°F

@Temperature 1500 °F
8 pcf
0.250 W/m-K

@Temperature 816 °C
1.74 BTU-in/hr-ft²-°F

@Temperature 1500 °F
6 pcf
0.260 W/m-K

@Temperature 982 °C
1.80 BTU-in/hr-ft²-°F

@Temperature 1800 °F
8 pcf
0.300 W/m-K

@Temperature 1093 °C
2.08 BTU-in/hr-ft²-°F

@Temperature 1999 °F
8 pcf
0.320 W/m-K

@Temperature 982 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 1800 °F
6 pcf
0.330 W/m-K

@Temperature 816 °C
2.29 BTU-in/hr-ft²-°F

@Temperature 1500 °F
4 pcf
0.430 W/m-K

@Temperature 982 °C
2.98 BTU-in/hr-ft²-°F

@Temperature 1800 °F
4 pcf
Melting Point 1760 °C
3200 °F
Maximum Service Temperature, Air 1090 °C
2000 °F
Continuous
1260 °C
2300 °F
Rating
Component Elements Properties Metric English Comments
Al2O3 45 %
45 %
Alkalis 0.20 %
0.20 %
B2O3 0.080 %
0.080 %
CaO 0.10 %
0.10 %
Fe2O3 1.0 %
1.0 %
SiO2 50 - 55 %
50 - 55 %
TiO2 1.7 %
1.7 %
Descriptive Properties Value Comments
MgO Content trace
Water Leachable Elements on Surface of Fiber, PPM Boron, 40
Chlorine, <10
Fluorine, <5
Silicate, 125
Sodium, 40
Sulphur, 10