Thermal Ceramics Cerachrome Blanket

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Thermal Ceramics
Trade Name Cerachrome
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Thermal Ceramics Cerachrome Blanket.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Made from spun alumina-silica-chromia fiber, Cerachrome Blanket is well suited for hot face lining applications where higher temperatures are encountered, such as soaking pit covers, reheat and forging furnaces. Cerachrome Blanket with its chromia-stabilized chemistry offers improved long term shrinkage characteristics over zirconia containing blankets such as Cerachem. Cerachrome Blanket effectively fills the gap between zirconia blankets and high alumina products.Military Specifications and Approvals:Mil-I-23128A- 3, 6 pcf blanketMil-I-24244- all blanketsMil-I-23128B- 6, 8 pcf blanketInformation provided by Thermal CeramicsData has not been recently verified. Please contact manufacturer for current information.
Physical Properties Metric English Comments
Density 0.0640 g/cc
0.00231 lb/in³
Available in multiple densities from manufacturer
0.0960 g/cc
0.00347 lb/in³
Available in multiple densities from manufacturer
0.128 g/cc
0.00462 lb/in³
Available in multiple densities from manufacturer
Thickness 12500 - 50000 microns
492 - 1970 mil
Thermal Properties Metric English Comments
Thermal Conductivity 0.0600 W/m-K

@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 500 °F
8 pcf
0.0700 W/m-K

@Temperature 260 °C
0.486 BTU-in/hr-ft²-°F

@Temperature 500 °F
6 pcf
0.0800 W/m-K

@Temperature 260 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 500 °F
4 pcf
0.130 W/m-K

@Temperature 538 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1000 °F
8 pcf
0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
6 pcf
0.190 W/m-K

@Temperature 538 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1000 °F
4 pcf
0.230 W/m-K

@Temperature 816 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 1500 °F
8 pcf
0.270 W/m-K

@Temperature 816 °C
1.87 BTU-in/hr-ft²-°F

@Temperature 1500 °F
6 pcf
0.300 W/m-K

@Temperature 982 °C
2.08 BTU-in/hr-ft²-°F

@Temperature 1800 °F
8 pcf
0.340 W/m-K

@Temperature 1093 °C
2.36 BTU-in/hr-ft²-°F

@Temperature 1999 °F
8 pcf
0.350 W/m-K

@Temperature 982 °C
2.43 BTU-in/hr-ft²-°F

@Temperature 1800 °F
6 pcf
0.360 W/m-K

@Temperature 816 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1500 °F
4 pcf
0.410 W/m-K

@Temperature 1093 °C
2.85 BTU-in/hr-ft²-°F

@Temperature 1999 °F
6 pcf
0.470 W/m-K

@Temperature 982 °C
3.26 BTU-in/hr-ft²-°F

@Temperature 1800 °F
4 pcf
0.540 W/m-K

@Temperature 1093 °C
3.75 BTU-in/hr-ft²-°F

@Temperature 1999 °F
4 pcf
Melting Point 1760 °C
3200 °F
Maximum Service Temperature, Air 1370 °C
2500 °F
Continuous
1430 °C
2600 °F
Rating
Component Elements Properties Metric English Comments
Al2O3 43 %
43 %
Cr2O3 3.0 %
3.0 %
SiO2 54 %
54 %
Descriptive Properties Value Comments
Other Element Content traces
Water Leachable Elements on Surface of Fiber, PPM Boron, 40
Chlorine, <10
Fluorine, <5
Silicate, 125
Sodium, 40
Sulphur, 10