Material Notes:
Cerachem Blanket is a 2600°F (1427°C) maximum temperature rated refractory blanket formed from a unique, patented, spun alumina-silica-zirconia fiber. It is specially designed for applications where high fiber tensile strength, low thermal conductivity and low shrinkage are required. Cerachem Blanket is used extensively in high temperature units in the ceramic, chemical processing, and ferrous metal industries. Thermal Ceramics Cerachem refractory blankets are ideal for a wide range of hot face lining and backup insulation applications in furnaces, kilns and other high temperature equipment. Military Specifications and Approvals:Mil-I-23128A- 3, 6 pcf blanketMil-I-24244- all blanketsMil-I-23128B- 6, 8 pcf blanketInformation provided by Thermal CeramicsData has not been recently verified. Please contact manufacturer for current information.
Physical Properties Metric English Comments
Density 0.0640 g/cc
0.00231 lb/in³
Available in multiple densities from manufacturer
0.0960 g/cc
0.00347 lb/in³
Available in multiple densities from manufacturer
0.128 g/cc
0.00462 lb/in³
Available in multiple densities from manufacturer
Thickness 12500 - 50000 microns
492 - 1970 mil
Thermal Properties Metric English Comments
Thermal Conductivity 0.0600 W/m-K

@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 500 °F
8 pcf
0.0700 W/m-K

@Temperature 260 °C
0.486 BTU-in/hr-ft²-°F

@Temperature 500 °F
6 pcf
0.0800 W/m-K

@Temperature 260 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 500 °F
4 pcf
0.130 W/m-K

@Temperature 538 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1000 °F
8 pcf
0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
6 pcf
0.190 W/m-K

@Temperature 538 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1000 °F
4 pcf
0.230 W/m-K

@Temperature 816 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 1500 °F
8 pcf
0.270 W/m-K

@Temperature 816 °C
1.87 BTU-in/hr-ft²-°F

@Temperature 1500 °F
6 pcf
0.300 W/m-K

@Temperature 982 °C
2.08 BTU-in/hr-ft²-°F

@Temperature 1800 °F
8 pcf
0.340 W/m-K

@Temperature 1093 °C
2.36 BTU-in/hr-ft²-°F

@Temperature 1999 °F
8 pcf
0.350 W/m-K

@Temperature 982 °C
2.43 BTU-in/hr-ft²-°F

@Temperature 1800 °F
6 pcf
0.360 W/m-K

@Temperature 816 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1500 °F
4 pcf
0.410 W/m-K

@Temperature 1093 °C
2.85 BTU-in/hr-ft²-°F

@Temperature 1999 °F
6 pcf
0.470 W/m-K

@Temperature 982 °C
3.26 BTU-in/hr-ft²-°F

@Temperature 1800 °F
4 pcf
0.540 W/m-K

@Temperature 1093 °C
3.75 BTU-in/hr-ft²-°F

@Temperature 1999 °F
4 pcf
Melting Point 1760 °C
3200 °F
Maximum Service Temperature, Air 1320 °C
2400 °F
Continuous
1430 °C
2600 °F
Rating
Component Elements Properties Metric English Comments
Al2O3 35 %
35 %
Alkalis 0.20 %
0.20 %
CaO 0.050 %
0.050 %
Fe2O3 0.050 %
0.050 %
MgO 0.050 %
0.050 %
SiO2 50 %
50 %
ZrO2 15 %
15 %
Descriptive Properties Value Comments
Other Element Content traces
Water Leachable Elements on Surface of Fiber, PPM Boron, 40
Chlorine, <10
Fluorine, <5
Silicate, 125
Sodium, 40
Sulphur, 10
Copyright © lookpolymers.com All Rights Reserved