Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Thermal Ceramics Cerablanket Blanket

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Thermal Ceramics
Trade Name Cerablanket
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Thermal Ceramics Cerablanket Blanket.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on average the highest tensile strength of any Thermal Ceramics ceramic fiber blanket. Cerablanket is available in a wide variety of densities and sizes. Cerablanket offers excellent handleability and high temperature stability which allows it to meet a wide range of hot face and back up insulation applications in furnaces, kilns and other equipment requiring high temperature heat containment.Military Specifications and Approvals:Mil-I-23128A- 3, 6 pcf blanketMil-I-24244- all blanketsMil-I-23128B- 6, 8 pcf blanketInformation provided by Thermal CeramicsData has not been recently verified. Please contact manufacturer for current information.
Physical Properties Metric English Comments
Density 0.0480 g/cc
0.00173 lb/in³
Available in multiple densities from manufacturer
0.0640 g/cc
0.00231 lb/in³
Available in multiple densities from manufacturer
0.0960 g/cc
0.00347 lb/in³
Available in multiple densities from manufacturer
0.128 g/cc
0.00462 lb/in³
Available in multiple densities from manufacturer
Thickness 6250 - 50000 microns
246 - 1970 mil
Thermal Properties Metric English Comments
Thermal Conductivity 0.0600 W/m-K

@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 500 °F
8 pcf
0.0700 W/m-K

@Temperature 260 °C
0.486 BTU-in/hr-ft²-°F

@Temperature 500 °F
6 pcf
0.0800 W/m-K

@Temperature 260 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 500 °F
4 pcf
0.130 W/m-K

@Temperature 538 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1000 °F
8 pcf
0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
6 pcf
0.190 W/m-K

@Temperature 538 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1000 °F
4 pcf
0.230 W/m-K

@Temperature 816 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 1500 °F
8 pcf
0.270 W/m-K

@Temperature 816 °C
1.87 BTU-in/hr-ft²-°F

@Temperature 1500 °F
6 pcf
0.300 W/m-K

@Temperature 982 °C
2.08 BTU-in/hr-ft²-°F

@Temperature 1800 °F
8 pcf
0.340 W/m-K

@Temperature 1093 °C
2.36 BTU-in/hr-ft²-°F

@Temperature 1999 °F
8 pcf
0.350 W/m-K

@Temperature 982 °C
2.43 BTU-in/hr-ft²-°F

@Temperature 1800 °F
6 pcf
0.360 W/m-K

@Temperature 816 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 1500 °F
4 pcf
0.410 W/m-K

@Temperature 1093 °C
2.85 BTU-in/hr-ft²-°F

@Temperature 1999 °F
6 pcf
0.470 W/m-K

@Temperature 982 °C
3.26 BTU-in/hr-ft²-°F

@Temperature 1800 °F
4 pcf
0.540 W/m-K

@Temperature 1093 °C
3.75 BTU-in/hr-ft²-°F

@Temperature 1999 °F
4 pcf
Melting Point 1760 °C
3200 °F
Maximum Service Temperature, Air 1180 °C
2150 °F
Continuous
1320 °C
2400 °F
Rating
Component Elements Properties Metric English Comments
Al2O3 46 %
46 %
Alkalis 0.20 %
0.20 %
CaO 0.050 %
0.050 %
Fe2O3 0.050 %
0.050 %
MgO 0.050 %
0.050 %
SiO2 54 %
54 %
Descriptive Properties Value Comments
Other Element Content traces
Water Leachable Elements on Surface of Fiber, PPM Boron, 40
Chlorine, <10
Fluorine, <5
Silicate, 125
Sodium, 40
Sulphur, 10
Copyright © lookpolymers.com All Rights Reserved