Category | Ceramic |
Manufacturer | Thermal Ceramics |
Trade Name | |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Thermal Ceramics 400-LS Mineral Fiber Paper.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.144 - 0.208 g/cc | 0.00520 - 0.00751 lb/in³ | |
Loss On Ignition | 5.0 - 10 % | 5.0 - 10 % |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.0345 - 0.0689 MPa | 5.00 - 10.0 psi | Fired |
0.276 - 0.517 MPa | 40.0 - 75.0 psi |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0519 W/m-K @Temperature 260 °C |
0.360 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
0.0836 W/m-K @Temperature 538 °C |
0.580 BTU-in/hr-ft²-°F @Temperature 1000 °F |
||
0.111 W/m-K @Temperature 704 °C |
0.770 BTU-in/hr-ft²-°F @Temperature 1300 °F |
||
Melting Point | 1090 °C | 2000 °F | |
Maximum Service Temperature, Air | 732 °C | 1350 °F |
Component Elements Properties | Metric | English | Comments |
---|---|---|---|
Al2O3 | 15 % | 15 % | |
CaO | 20 % | 20 % | |
Other | 22 % | 22 % | |
SiO2 | 43 % | 43 % |