The NanoSteel® Company SHS 9500 GMAW OAW Steel Alloy, Cored Wire

Category Metal , Ferrous Metal , Alloy Steel , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer The NanoSteel® Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF The NanoSteel® Company SHS 9500 GMAW OAW Steel Alloy, Cored Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Coating Description: SHS 9500 GMAW OAW is an iron based steel alloy featuring medium hardness, high toughness and high wear resistance.Key Performance Characteristics: 58-62 HRc single and double pass weld depositsMinimal cracking when applied to plain carbon and alloy steelsCost effective: contains no tungsten, molybdenum or nickelHigh resistance to abrasion and galling SHS GMAW OAW features a unique uniform glass-forming melt chemistry that allows high undercooling to be achieved during welding. This results in considerable refinement of the crystalline microstructure down to a near nanoscale (400 nm length scale) range. Application Process: GMAW OAW Weld Overlay for HardfacingInformation Provided by The NanoSteel Company, Inc.
Physical Properties Metric English Comments
Density 7.59 g/cc
0.274 lb/in³
Weld Deposit Property
Mechanical Properties Metric English Comments
Hardness, Rockwell C 58 - 62
58 - 62
Component Elements Properties Metric English Comments
Boron, B <= 6.0 %
<= 6.0 %
Carbon, C <= 3.0 %
<= 3.0 %
Chromium, Cr <= 10 %
<= 10 %
Iron, Fe >= 65 %
>= 65 %
Manganese, Mn <= 5.0 %
<= 5.0 %
Niobium, Nb (Columbium, Cb) <= 9.0 %
<= 9.0 %
Silicon, Si <= 2.0 %
<= 2.0 %
Descriptive Properties Value Comments
Impact Resistance Passed multiple impacts at 165 ft-lbs
Drop Impact Testing
Wear Resistance Mass Loss (g) 0.19-0.25
6000 cycles; ASTM G65-04 Procedure A