The NanoSteel® Company SHS 9172 HVOF Steel Alloy, Atomized Powder

Category Metal , Ferrous Metal , Alloy Steel , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer The NanoSteel® Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF The NanoSteel® Company SHS 9172 HVOF Steel Alloy, Atomized Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Coating Description: SHS 9172 HVOF is an iron based steel alloy with a nanoscale microstructure that features exceptional resistance to wear, abrasion, impact, corrosion and high temperature oxidation. SHS 9172 HVOF is also a coating alternative to electrolytic hard chromium.Key Performance CharacteristicsExceptional abrasion resistance for a metallic materialSignificant corrosion and high temperature oxidation resistanceCoatings provide hardness, corrosion and wear resistance superior to hard chromeCan be finished to very high surface specifications as a replacement for hard chromeApplication Process: High Velocity Oxygen Fuel (HVOF) thermal sprayingInformation Provided by The NanoSteel Company, Inc.
Physical Properties Metric English Comments
Density 7.59 g/cc
0.274 lb/in³
Coating Property
Porosity <= 5.0 %
<= 5.0 %
Coating Property
Mechanical Properties Metric English Comments
Vickers Microhardness 1000 - 1100
1000 - 1100
kg/mm<sup>2</sup>; HV300
Component Elements Properties Metric English Comments
Boron, B <= 5.0 %
<= 5.0 %
Carbon, C <= 4.0 %
<= 4.0 %
Chromium, Cr <= 25 %
<= 25 %
Iron, Fe >= 28 %
>= 28 %
Manganese, Mn <= 3.0 %
<= 3.0 %
Molybdenum, Mo <= 6.0 %
<= 6.0 %
Niobium, Nb (Columbium, Cb) <= 12 %
<= 12 %
Silicon, Si <= 2.0 %
<= 2.0 %
Tungsten, W <= 15 %
<= 15 %
Descriptive Properties Value Comments
Impact Resistance No delamination/cracking at 480 in-lbs
Drop Impact Testing
Wear Resistance Mass Loss (g) 0.07
2000 cycles; ASTM G65-04 Procedure B