Terio Corporation TZOH-50 Zirconium Hydroxide

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer Terio Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Terio Corporation TZOH-50 Zirconium Hydroxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by TERIO Corporation.
Physical Properties Metric English Comments
Particle Size 2.0 - 50 µm
2.0 - 50 µm
PSD (d<sub>50</sub>
Specific Surface Area 10 - 300 m²/g
10 - 300 m²/g
Component Elements Properties Metric English Comments
ZrO2 50 %
50 %