Ter Hell Plastic Terez® PC X 9005 GF 5 Polycarbonate, 5% Glass Fiber

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled
Manufacturer Ter Hell Plastic GMBH
Trade Name Terez®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ter Hell Plastic Terez® PC X 9005 GF 5 Polycarbonate, 5% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polycarbonate, medium flowability, 5% glass fiber reinforced.Application: For injection molded parts with increased demand of stiffness.Information provided by Ter Hell Plastic GMBH.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ISO 1183
Water Absorption 0.32 %
0.32 %
ISO 62
Melt Flow 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength 60.0 MPa
8700 psi
dry; ISO 527
Tensile Strength, Yield 65.0 MPa
9430 psi
dry; ISO 527
Elongation at Break 20 %
20 %
dry; ISO 527
Elongation at Yield 5.0 %
5.0 %
dry; ISO 527
Tensile Modulus 3.00 GPa
435 ksi
dry; ISO 527
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
dry; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
ISO 75
Vicat Softening Point 135 °C
275 °F
B/50; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Processing Properties Metric English Comments
Processing Temperature 270 - 300 °C
518 - 572 °F
Drying Temperature 120 °C
248 °F
Dry Time 4 hour
4 hour