Ter Hell Plastic Terez® PBT 6750 T Polybutylene Terephthalate, Impact Modified

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Impact Grade
Manufacturer Ter Hell Plastic GMBH
Trade Name Terez®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ter Hell Plastic Terez® PBT 6750 T Polybutylene Terephthalate, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Impact modified PBT.Application: For impact stressed, injection molding parts.Information provided by Ter Hell Plastic GMBH.
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ISO 1183
Water Absorption 0.35 %
0.35 %
ISO 62
Moisture Absorption at Equilibrium 0.14 %
0.14 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength 60.0 MPa
8700 psi
dry; ISO 527
Tensile Strength, Yield 42.0 MPa
6090 psi
dry; ISO 527
Elongation at Break 15 %
15 %
dry; ISO 527
Elongation at Yield 5.0 %
5.0 %
dry; ISO 527
Tensile Modulus 2.10 GPa
305 ksi
dry; ISO 527
Charpy Impact Unnotched NB
NB
dry; ISO 179
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
dry; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 165 °C
329 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093
Comparative Tracking Index 450 V
450 V
IEC 60112
Processing Properties Metric English Comments
Processing Temperature 230 - 270 °C
446 - 518 °F
Drying Temperature 100 °C
212 °F
Dry Time 6 hour
6 hour